Surfaces should be clean, sound and free from contamination. Remove loose materials and repair honeycombing or deteriorated concrete with suitable low permeability repair mortar
Priming
No primer required, but substrates should be pre-soaked with clean water prior to application
Mixing
Add 3 kg liquid into a clean container, slowly add 17 kg powder while mixing at 300-400 rpm and continue for 3 minutes until uniform
Application
Apply by roller, brush or spray. Brush the material well into the surface and avoid spreading too thin
Waterproofing behind stone veneer and exterior cladding
Protection of concrete and masonry against carbon dioxide, chloride ions, water and de-icing salts
Waterproofing wet areas such as bathrooms and kitchens
Waterproofing water retaining structures and reservoirs